PA66 Zytel® HTN51G35HSLR BK420J DUPONT USA
128
Unit Price:$8155 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced|Thermal stability|Flame retardant|High temperature resistan|Food contact compliance
- Application Areas:Automotive interior parts|Electrical appliances|Fitness equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Moisture Absorption | 饱和,23°C,2.00mm | ISO62 | 4.5 % |
Modeling Shrinkage | TD | ISO294-4 | 0.60 % |
MD | ISO294-4 | 0.20 % | |
SpecificHeatCapacityofMelt | 1860 J/kg/°C | ||
ThermalConductivityofMelt | 0.25 W/m/K |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,未退火 | ISO75-2/B | 284 °C |
1.8MPa,未退火 | ISO75-2/A | 260 °C | |
Melting Temperature | ISO11357-3 | 300 °C | |
Linear thermal expansion coefficient | MD:-- | ISO11359-2 | 1.8E-05 cm/cm/°C |
MD:-40to23°C | ISO11359-2 | 1.8E-05 cm/cm/°C | |
TD:-- | ISO11359-2 | 5.5E-05 cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 5.5E-05 cm/cm/°C |
Additional | Test Condition | Test Method | Test Result |
---|---|---|---|
Odor | VDA270 | 4.00 |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Burning Rate | 1.00mm | ISO3795 | 23 mm/min |
Flame Rating | 0.9mm | UL94 | HB |
1.5mm | UL94 | HB | |
0.9mm | IEC60695-11-10,-20 | HB | |
1.5mm | IEC60695-11-10,-20 | HB | |
Oxygen Index | ISO4589-2 | 24 % | |
FMVSS Flammability | FMVSS302 | B |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Modulus | ISO527-2 | 12000 Mpa | |
Tensile Stress | 断裂 | ISO527-2 | 210 Mpa |
Tensile Strain | 断裂 | ISO527-2 | 2.4 % |
Tensile Creep Modulus | 1hr | ISO899-1 | -- Mpa |
1000hr | ISO899-1 | -- Mpa | |
Flexural Modulus | ISO178 | 10300 Mpa | |
Flexural Stress | ISO178 | 300 Mpa | |
Poisson Ratio | ISO527 | 0.39 |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Comparative Tracking Index | IEC60112 | 600 V | |
Surface Resistivity | IEC60093 | -- ohms | |
Volume Resistivity | IEC60093 | >1.0E+15 ohms·cm | |
Dielectric Strength | IEC60243-1 | 36 KV/mm | |
Relative Permittivity | 100Hz | IEC60250 | 4.00 |
1MHz | IEC60250 | 4.00 |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | M计秤 | ISO2039-2 | 108 |
R计秤 | ISO2039-2 | 124 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 60 kJ/m² |
23°C | ISO179/1eU | 70 kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.