Need Help? Contact Us service@plas.com
Get App

PA66 LNP™ LUBRICOMP™  RL-4540 RD SABIC INNOVATIVE US

92
  • Unit Price:
    $3536 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Thermal stability wear resistant
  • Application Areas:Electronic and Electrical Automotive External Parts
  • Color:--
  • Grade:Impact resistant grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9551.0to3.0%
Shrinkage rateTD:24hrASTMD9551.0to3.0%
Water absorption rate24hr,50%RHASTMD5700.84%
Water absorption rateEquilibrium,23°C,50%RHISO621.1%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile stressYieldISO527-2/563.0Mpa
Tensile stressBreakISO527-2/563.0Mpa
Tensile strainYieldISO527-2/526%
Tensile strainBreakISO527-2/527%
Tensile modulusISO527-2/12730Mpa
friction coefficientDynamicASTMD3702Modified0.020
friction coefficientStaticASTMD3702Modified0.045
Elongation rate 3YieldASTMD63822%
Tensile modulus 2ASTMD6382620Mpa
Tensile strength 3YieldASTMD63861.0Mpa
Tensile strength 3BreakASTMD63861.0Mpa
Bending modulus 450.0mmSpanASTMD7902260Mpa
Elongation rate 4BreakASTMD63823%
Bending modulus 5ISO1782400Mpa
Wear factor - WasherASTMD3702Modified3.5010^-10in^5-min/ft-lb-hr
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature 71.8MPa,Unannealed,64.0mmSpanISO75-2/Af63.0°C
Hot deformation temperature 70.45MPa,Unannealed,64.0mmSpanISO75-2/Bf200°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTMD648237°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD64864.0°C
Linear coefficient of thermal expansionMD:-30to30°CASTMD6968.4E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTMD6969.4E-05cm/cm/°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Multi axis Instrumented Impact EnergyISO6603-21.20J
Dart impact equipped with measuring instruments23°C,TotalEnergyASTMD37636.70J
Suspended wall beam notch impact strength 623°CISO180/1A5.2kJ/m²
Unscented Izod Impact Strength 523°CISO180/1U88kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.