PA66 Amilan® CM1011G45 TORAY JAPAN
125
- Unit Price:
- $3239 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 76.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High impact resistance Glass fiber reinforced Glass 45% reinforced High modulus application High impact Glass 45% reinforced High modulus application High impact
- Application Areas:Automotive sector
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ASTM D-792 | 无水|1.5 | ||
ASTM D-792 | 1.9%水|- | |||
Taber wear amount | 1000g,CS-17 | ASTM D-1044 | 无水|30 | mg/1000次 |
1000g,CS-17 | ASTM D-1044 | 1.9%水|- | mg/1000次 |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
elongation at break | 23℃ | ASTM D-638 | 无水|5 | % |
23℃ | ASTM D-638 | 1.9%水|5 | % | |
Flexural modulus | 23℃ | ASTM D-790 | 无水|122000 | kg/cm2 |
23℃ | ASTM D-790 | 1.9%水|72000 | kg/cm2 | |
80℃ | ASTM D-790 | 无水|63000 | kg/cm2 | |
80℃ | ASTM D-790 | 1.9%水|45000 | kg/cm2 | |
-40℃ | ASTM D-790 | 无水|140000 | kg/cm2 | |
-40℃ | ASTM D-790 | 1.9%水|120000 | kg/cm2 | |
Rockwell hardness | 23℃ | ASTM D-785 | 无水|95 | M-标度 |
23℃ | ASTM D-785 | 1.9%水|- | M-标度 | |
23℃ | ASTM D-785 | 无水|121 | R-标度 | |
Flexural strength | 23℃ | ASTM D-790 | 无水|2900 | kg/cm2 |
23℃ | ASTM D-790 | 1.9%水|1850 | kg/cm2 | |
80℃ | ASTM D-790 | 无水|16000 | kg/cm2 | |
80℃ | ASTM D-790 | 1.9%水|- | kg/cm2 | |
-40℃ | ASTM D-790 | 无水|3300 | kg/cm2 | |
-40℃ | ASTM D-790 | 1.9%水|- | kg/cm2 | |
Tensile yield strength | 23℃ | ASTM D-638 | 无水|2000 | kg/cm2 |
23℃ | ASTM D-638 | 1.9%水|1300 | kg/cm2 | |
80℃ | ASTM D-638 | 无水|1200 | kg/cm2 | |
80℃ | ASTM D-638 | 1.9%水|- | kg/cm2 | |
-40℃ | ASTM D-638 | 无水|2900 | kg/cm2 | |
-40℃ | ASTM D-638 | 1.9%水|- | kg/cm2 | |
compressive strength | 23℃ | ASTM D-695 | 无水|1900 | kg/cm2 |
23℃ | ASTM D-695 | 1.9%水|- | kg/cm2 | |
80℃ | ASTM D-695 | 无水|1000 | kg/cm2 | |
80℃ | ASTM D-695 | 1.9%水|- | kg/cm2 | |
-40℃ | ASTM D-695 | 无水|2600 | kg/cm2 | |
-40℃ | ASTM D-695 | 1.9%水|- | kg/cm2 | |
Shear strength | 23℃ | ASTM D-732 | 无水|940 | kg/cm2 |
23℃ | ASTM D-732 | 1.9%水|750 | kg/cm2 | |
Rockwell hardness | 23℃ | ASTM D-785 | 1.9%水|- | R-标度 |
IZOD impact strength | 23℃,Unnotched1/8 | ASTM D-256 | 1.9%水|120 | kg·cm/cm |
-40℃,Unnotched1/8 | ASTM D-256 | 无水|12.5 | kg·cm/cm | |
-40℃,Unnotched1/8 | ASTM D-256 | 1.9%水|15 | kg·cm/cm | |
-40℃,Unnotched1/8 | ASTM D-256 | 无水|12.5 | kg·cm/cm2 | |
-40℃,Unnotched1/8 | ASTM D-256 | 1.9%水|15 | kg·cm/cm2 | |
23℃,VNotched1/2 | ASTM D-256 | 无水|15 | kg·cm/cm | |
23℃,VNotched1/2 | ASTM D-256 | 1.9%水|20 | kg·cm/cm | |
23℃,Unnotched1/8 | ASTM D-256 | 无水|98 | kg·cm/cm |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
heat deflection temperature | 4.6kg/cm2 | ASTM D-648 | 无水|225 | °C |
4.6kg/cm2 | ASTM D-648 | 1.9%水|- | °C | |
melting point | 差示扫描测热计DSC | 无水|225 | °C | |
差示扫描测热计DSC | 1.9%水|- | °C | ||
specific heat | 无水|0.31 | Cal/g·℃ | ||
1.9%水|- | Cal/g·℃ | |||
Linear coefficient of thermal expansion | ASTM D-696 | 无水|2-3 | ×10-5cm/cm/℃ | |
ASTM D-696 | 1.9%水|- | ×10-5cm/cm/℃ | ||
UL-94 flame retardant grade | 1/32" | UL 94 | 无水|HB | |
1/32" | UL 94 | 1.9%水|- |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Arc resistance | 1/8" | ASTM D-495 | 无水|104 | S |
1/8" | ASTM D-495 | 1.9%水|119 | S | |
Loss factor | 106Hz | ASTM D-150 | 无水|0.02 | |
106Hz | ASTM D-150 | 1.9%水|0.06 | ||
Dielectric strength | 1/8" | ASTM D-149 | 无水|19 | KV/mm |
1/8" | ASTM D-149 | 1.9%水|15 | KV/mm | |
Dielectric constant | 106Hz | ASTM D-150 | 无水|4.2 | |
106Hz | ASTM D-150 | 1.9%水|4.5 | ||
103Hz | ASTM D-150 | 无水|4.9 | ||
103Hz | ASTM D-150 | 1.9%水|7.4 | ||
Volume resistivity | ASTM D-257 | 无水|1015 | Ω.cm | |
ASTM D-257 | 1.9%水|1012 | Ω.cm | ||
Loss factor | 50Hz | ASTM D-150 | 无水|0.03 | |
50Hz | ASTM D-150 | 1.9%水|0.16 |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Enhanced content | 无水|45 | wt% | ||
1.9%水|- | wt% |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | 23℃,24hr | ASTM D-570 | 无水|0.9 | % |
23℃,24hr | ASTM D-570 | 1.9%水|- | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.