PA66 Leona™ 1402G BK ASAHI JAPAN
107
- Unit Price:
- $3393 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 54MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High rigidity high strength Fatigue resistance Creep resistance Thermal stability Moderate heat resistance
- Application Areas:Electrical field Electronic field component Automotive sector
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ASTM D792, ISO 1183 | 1.39 | g/cm³ | |
Shrinkage rate | Across Flow | 内部方法 | 0.90 | % |
流量 | 内部方法 | 0.40 | % | |
Water absorption rate | Saturation, 23°C | -- | % | |
Equilibrium, 23°C, 50% RH | ISO 62 | -- | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | 23°C | ISO 527-2 | 10000 | Mpa |
Tensile stress | Break, 23°C | ISO 527-2 | 190 | Mpa |
-- | ASTM D638 | 186 | Mpa | |
elongation | Break | ASTM D638 | 3.0 | % |
Break, 23°C | ISO 527-2 | 3.0 | % | |
Bending modulus | -- | ASTM D790 | 9300 | Mpa |
23°C | ISO 178 | 9000 | Mpa | |
bending strength | -- | ASTM D790 | 289 | Mpa |
23°C | ISO 178 | 275 | Mpa | |
Taber abraser | 1000 Cycles | ASTM D1044 | -- | mg |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Thermal deformation temperature under load | 0.45 MPa, Unannealed | ASTM D648 | 260 | °C |
0.45 MPa, Unannealed | ISO 75-2/B | 265 | °C | |
1.8 MPa, Unannealed | ASTM D648, ISO 75-2/A | 250 | °C | |
Linear coefficient of thermal expansion - flow | ASTM D696 | 3.0E-5 | cm/cm/°C | |
specific heat | 1590 | J/kg/°C | ||
thermal conductivity | 0.30 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTM D257, IEC 60093 | 1.0E+15 | ohms | |
Volume resistivity | -- | ASTM D257 | 1.0E+15 | ohms·cm |
23°C | IEC 60093 | 1.0E+15 | ohms·cm | |
Dielectric strength | ASTM D149, IEC 60243-1 | 28 | KV/mm | |
Leakage Trace Index | 3.00 mm | IEC 60112 | 425 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | 11 | kJ/m² | |
Impact strength of simply supported beam without notch | ISO 179 | 72 | kJ/m² | |
Impact strength of cantilever beam gap | ASTM D256 | 130 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | M-Scale | ASTM D785 | 96 | |
R-Scale | ASTM D785 | 120 | ||
M -Sale | ISO 2039-2 | 96 | ||
R -Sale | ISO 2039-2 | 120 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.75 mm | UL 94 | HB | |
Extreme Oxygen Index | ASTM D2863 | 23 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.