PA66 Zytel® 70G35HSL DUPONT USA
107
- Unit Price:
- $3942 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 144.9MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability wear resistant Filler: Glass fiber reinf 35% filler by weight
- Application Areas:Electronic appliances Home appliance components Connector
- Color:--
- Grade:Enhanced level
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD2.0mm | ISO294-4 | 0.30 | % |
TD2.0mm | ISO294-4 | 1.10 | % | |
Density/specific gravity | ISO1183 | 1.41 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 90 | kJ/m² |
-30°C | ISO179/1eU | 80 | kJ/m² | |
Tensile creep modulus | 1Hr | ISO899-1 | Mpa | |
1000Hr | ISO899-1 | Mpa | ||
elongation at break | 23°C | ISO527-2 | 3.20 | % |
Tensile modulus | 23°C | ISO527-2 | 11200 | Mpa |
tensile strength | 23°C | ISO527-2 | 210 | Mpa |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 15 | kJ/m² |
-30°C | ISO179/1eA | 10 | kJ/m² | |
Impact strength of cantilever beam gap | 23°C | ISO180/1A | 12 | kJ/m² |
-30°C | ISO180/1A | 10 | kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat softening temperature | ISO306/B50 | 255 | °C | |
玻璃转化温度 | ISO11357-2 | 80 | °C | |
Melting Temperature | ISO11357-3 | 262 | °C | |
Hot deformation temperature | 0.45MPaUnannealed | ISO75-2/Bf | 261 | °C |
1.80MPaAnnealed | ISO75-2/Af | 252 | °C | |
Coefficient of linear expansion | MD | ISO11359-2 | 2E-05 | cm/cm/°C |
TD | ISO11359-2 | 1E-04 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Insulation strength | IEC60243-1 | 33 | KV/mm | |
Volume resistance | IEC60093 | 1E+13 | Ω.cm | |
Dissipation factor | 相对漏电起痕指数 | IEC60112 | 400 | V |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | ISO2039-2 | 105 | M(Scale) | |
ISO2039-2 | 125 | R |
Flame retardant performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Fire rating | UL-94 | 0.71mm | HB | |
UL-94 | 1.50mm | HB | ||
UL-94 | 3.00mm | HB | ||
氧指数 | ISO4589-2 | 24 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.