PA6 6G50AFH BK DOMO CHEM GERMANY
204
- Unit Price:
- $2981 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 91MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability UV resistance Glass fiber reinforced Filler glass fiber reinf
- Application Areas:--
- Color:--
- Grade:Enhanced level
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:23°C,72小时 | ISO2577 | 0.10to0.20 | % |
Stickiness number | ISO307 | 125 | cm³/g | |
density | ISO1183 | 1.56 | g/cm³ | |
Shrinkage rate | TD:23°C,72小时 | ISO2577 | 0.40to0.60 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2/1 | 15500 | Mpa | |
Tensile stress | 断裂 | ISO527-2/5 | 210 | Mpa |
Tensile strain | 断裂 | ISO527-2/5 | 2.0 | % |
Bending modulus | ISO178 | 14000 | Mpa | |
Bending stress | ISO178 | 320 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,未退火 | ISO75-2/B | 220 | °C |
1.8MPa,未退火 | ISO75-2/A | 210 | °C | |
Vicat softening temperature | ISO306/B50 | 215 | °C | |
Melting temperature | ISO11357-3 | 222 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | IEC60093 | 1E+13 | ohms | |
Volume resistivity | IEC60093 | 1E+15 | ohms·cm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Unscented Izod impact strength | 23°C | ISO180/1U | 90 | kJ/m² |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 20 | kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 95 | kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO180/1A | 19 | kJ/m² |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning rate | FMVSS302 | <100 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.