PA6 Ultramid® B3GM35 BASF GERMANY
168
Unit Price:$3022 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Oil resistant dimensional stability Medium hardness Filler: Glass mineral 40% filler by weight
- Application Areas:Phone case Industrial components Automotive sector Industrial applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ASTMD792 | 1.48 | g/cm³ | |
ISO1183 | 1.48 | g/cm³ | ||
Shrinkage rate | MD:3.18mm | 0.40 | % | |
Water absorption rate | Saturation | ASTMD570 | 5.7 | % |
Saturation,23°C | ISO62 | 5.7 | % | |
Equilibrium,50%RH | ASTMD570 | 1.7 | % | |
Equilibrium,23°C,50%RH | ISO62 | 1.7 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | 23°C | ISO527-2 | 7960 | Mpa |
Tensile strength | Break,23°C | ASTMD638 | 123 | Mpa |
Tensile stress | Break,23°C | ISO527-2 | 123 | Mpa |
elongation | Break,23°C | ASTMD638 | 2.6 | % |
Tensile strain | Break,23°C | ISO527-2 | 2.7 | % |
Bending modulus | 23°C | ISO178 | 7500 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/A | 199 | °C |
Peak melting temperature | ASTMD3418 | 220 | °C | |
Melting temperature (DSC) | ISO3146 | 220 | °C | |
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 198 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179 | 4.1 | kJ/m² |
Impact strength of cantilever beam gap | -40°C | ASTMD256 | 40 | J/m |
23°C | ASTMD256 | 53 | J/m | |
23°C | ISO180 | 4.8 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.