PPO/PA NORYL GTX™ GTX914-94302 SABIC INNOVATIVE US
193
- Unit Price:
- $5481 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility dimensional stability High temperature resistan Hydrolysis resistance Excellent impact resistan Temperature resistance Chemical properties and p
- Application Areas:Electrical applications Industrial machinery
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
hardness | H358/30 | ISO 2039/1 | 90 | Mpa |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
tensile strength | 50mm/min,Yield | ISO 527 | 55 | Mpa |
50mm/min,Break | ISO 527 | 55 | Mpa | |
tensile elongation | 50mm/min,Yield | ISO 527 | 7.5 | % |
50mm/min,Break | ISO 527 | 60 | % | |
Tensile modulus | 1mm/min | ISO 527 | 2100 | Mpa |
bending strength | 2mm/min | ISO 178 | 80 | Mpa |
Bending modulus | 2mm/min | ISO 178 | 2000 | Mpa |
Charpy Notched Impact Strength | 23℃ | ISO 179/2C | 30 | KJ/m |
IZOD impact strength | 23℃ 有Notched | ISO 180/1A | 30 | KJ/m |
-30℃ 有Notched | ISO 180/1A | 15 | KJ/m |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Thermal conductivity coefficient | DIN 52612 | 0.23 | W/m℃ | |
Linear coefficient of thermal expansion | DIN 53752 | 9E-05 | 1/℃ | |
Vicat hot deformation temperature | A/50 | ISO 306 | 245 | °C |
B/50 | ISO 306 | 190 | °C | |
B/120 | ISO 306 | 195 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Electrical strength | IEC 243 | 20.0 | KV/mm | |
Electrical factor | 50Hz | IEC 250 | 0.0720 | |
1MHz | IEC 250 | 0.0240 |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen index | ISO 4589 | 21 | % |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ISO 1183 | 1.09 | g/cm | |
Water absorption rate | DIN 53495 | 3.50 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.