PBT/PET SCHULADUR® PCR GF 45 BK A SCHULMAN USA
261
Unit Price:$2283 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 28MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Filler: Glass fiber reinf 45% filler by weight
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
吸水率 | 平衡,23°C,50%RH | ISO62 | 0.25 | % |
熔体体积流动速率 | 260°C/2.16kg | ISO1133 | 11.0 | cm3/10min |
机械性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
拉伸应力 | 断裂 | ISO527-2/1A/5 | 160 | Mpa |
拉伸应变 | 断裂 | ISO527-2/1A/5 | 1.7 | % |
拉伸模量 | ISO527-2/1A/1 | 15500 | Mpa | |
弯曲模量2 | ISO178 | 16000 | Mpa | |
弯曲应力2 | ISO178 | 250 | Mpa |
热性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
热变形温度 | 0.45MPa,未退火 | ISO75-2/Bf | 225 | °C |
1.8MPa,未退火 | ISO75-2/Af | 208 | °C | |
维卡软化温度 | -- | ISO306/A50 | 214 | °C |
-- | ISO306/B50 | 198 | °C |
冲击性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
简支梁无缺口冲击强度 | -30°C | ISO179/1eU | 50 | kJ/m² |
23°C | ISO179/1eU | 50 | kJ/m² |
可燃性 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL阻燃等级 | 1.6mm | IEC60695-11-10,-20 | HB | |
3.2mm | IEC60695-11-10,-20 | HB | ||
灼热丝易燃指数 | 1.5mm | IEC60695-2-12 | 700 | °C |
3.0mm | IEC60695-2-12 | 800 | °C | |
热灯丝点火温度 | 1.5mm,Passes | IEC60695-2-13 | 825 | °C |
3.0mm,Passes | IEC60695-2-13 | 800 | °C | |
燃烧速率 | ISO3795 | 25 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.