ASA/PC GELOY™  XP4034-BK1041 SABIC INNOVATIVE NANSHA

246
  • Unit Price:
    $3478 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    43MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Thermal stability Weather resistance Antistatic High mobility
  • Application Areas:Automotive Applications
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Melt flow rate280°C/3.8 kgASTM D123824g/10 min
Shrinkage rateFlow : 3.20 mm内部方法0.50 到 0.70%
Shrinkage rateAcross Flow : 3.20 mm内部方法0.50 到 0.70%
Water absorption rate24 hrASTM D5700.25%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile strengthYieldASTM D63862.0Mpa
elongationBreakASTM D63825%
Bending modulus50.0 mm SpanASTM D7902510Mpa
bending strength Yield, 50.0 mm SpanASTM D79088.0Mpa
Thermal performanceTest ConditionTest MethodTest ResultUnit
Thermal deformation temperature under load0.45 MPa, Unannealed, 3.20 mmASTM D648115°C
Thermal deformation temperature under load1.8 MPa, Unannealed, 6.40 mmASTM D648104°C
Linear coefficient of thermal expansionFlow : -20 to 150°CASTM E8317.2E-5cm/cm/°C
Linear coefficient of thermal expansionAcross Flow : -20 to 150°CASTM E8317.2E-5cm/cm/°C
thermal conductivityASTM C1770.25W/m/K
injectionTest ConditionTest MethodTest ResultUnit
drying temperature95 到 105°C
drying time3.0 到 4.0hr
Suggested maximum moisture content0.040%
Suggested injection volume40 到 80%
Temperature at the rear of the barrel240 到 255°C
Temperature in the middle of the barrel245 到 260°C
Temperature at the front of the material cylinder250 到 265°C
Spray nozzle temperature245 到 265°C
Processing (melt) temperature260 到 275°C
Mold temperature55 到 70°C
Back pressure0.300 到 1.00Mpa
Screw speed30 到 80rpm
Exhaust hole depth0.038 到 0.076mm
Impact performanceTest ConditionTest MethodTest ResultUnit
Dart impact equipped with measuring instruments-30°C, Total EnergyASTM D376330.0J
Dart impact equipped with measuring instruments23°C, Total EnergyASTM D376347.0J
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell hardnessR-ScaleASTM D785110
optical performance Test ConditionTest MethodTest ResultUnit
Gardner glossiness60°, 无织构ASTM D52394
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.