EAA PRIMACOR™ 3004 STYRON US
275
- Unit Price:
- $3300 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 90MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Heat sealing performance High toughness Resistance to stress crac
- Application Areas:Cable Electric wire
- Color:--
- Grade:Extrusion grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | g/cm³ | ASTM D-792 | 0.938 | |
g/cm³ | ISO 1183 | 0.938 | ||
ASTMD792,ISO1183 | 0.938 | g/cm³ | ||
Melt mass flow rate 2 | 190°C/2.16kg | ASTMD1238,ISO1133 | 8.5 | g/10min |
Content of comonomer 3 | 9.7 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength | Yield,Compression Molded | ASTMD638,ISO527-2 | 7.93 | Mpa |
Break,Compression Molded | ASTMD638,ISO527-2 | 17.6 | Mpa | |
elongation | Break,Compression Molded | ASTMD638,ISO527-2 | 600 | % |
Tensile yield strength | Compression Molded | MPa | ASTM D-638 | 7.93 |
Compression Molded | MPa | ISO 527-2 | 7.93 | |
Tensile fracture strength | Compression Molded | MPa | ASTM D-638 | 17.6 |
Compression Molded | MPa | ISO 527-2 | 17.6 | |
Tensile strain at break | Compression Molded | % | ASTM D-638 | 600 |
Compression Molded | % | ISO 527-2 | 600 |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat softening temperature | ASTMD1525,ISO306 | 81.1 | °C | |
Melting temperature (DSC) | 内部方法 | 98.0 | °C | |
vicat softening point | ℃ | ASTM D-1525 | 81.1 | |
℃ | ISO 306 | 81.1 |
Processing performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Temperature | ℃ | 260-290 |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt index | 190℃/2.16kg | g/10min | ASTM D-1238 | 8.5 |
190℃/2.16kg | g/10min | ISO 1133 | 8.5 | |
Monomer content | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.