PSU UDEL® P-1710 NT15 SOLVAY USA
211
- Unit Price:
- $19618 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 17MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Hydrolysis resistance Chemical resistance
- Application Areas:Electrical components Electrical appliances Valves/valve components Industrial components Pipeline components Pipeline system Home appliance components parts Food service sector Microwave cooker
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 343°C/2.16kg | ASTMD1238 | 7.0 | g/10min |
Shrinkage rate | MD | ASTMD955 | 0.70 | % |
Water absorption rate | 24hr | ASTMD570 | 0.30 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ASTMD638 | 2480 | Mpa | |
Tensile strength | ASTMD638 | 70.3 | Mpa | |
elongation | Break | ASTMD638 | 50to100 | % |
Bending modulus | ASTMD790 | 2690 | Mpa | |
bending strength | ASTMD790 | 106 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear coefficient of thermal expansion | MD | ASTMD696 | 5.6E-05 | cm/cm/°C |
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 174 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | ASTMD257 | 5E+16 | ohms·cm | |
Dielectric strength | ASTMD149 | 17 | KV/mm | |
Dielectric constant | 60Hz | ASTMD150 | 3.15 | |
1kHz | ASTMD150 | 3.14 | ||
1MHz | ASTMD150 | 3.10 | ||
Dissipation factor | 60Hz | ASTMD150 | 1.1E-03 | |
1kHz | ASTMD150 | 1.3E-03 | ||
1MHz | ASTMD150 | 5E-03 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile impact strength | ASTMD1822 | 420 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.