TPU Texin® RxT85A 00000 COVESTRO GERMANY
121
- Unit Price:
- $19388 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 18MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Medical grade
- Application Areas:film catheter Washer Pipe fittings Connector Seals Profile Medical/nursing supplies
- Color:--
- Grade:Medical grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:2.54mm | ASTMD955 | 0.80 | % |
TD:2.54mm | ASTMD955 | 0.80 | % | |
TD:2.54mm | ISO2577 | 0.80 | % | |
MD:2.54mm | ISO2577 | 0.80 | % | |
Melt mass flow rate | 190°C/8.7kg | ASTMD1238 | 4.0 | g/10min |
190°C/8.7kg | ISO1133 | 4.0 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Taber abraser | 1000Cycles,1000g,H-18Wheel | ASTMD1044 | 30.0 | mg |
1000Cycles,1000g,H-18Wheel | ISO4649 | 30.0 | mg | |
Bending modulus | 23°C | ASTMD790 | 29.9 | Mpa |
23°C | ISO178 | 26.9 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat softening temperature | ASTMD15254 | 80.0 | °C | |
ISO306/50 | 80.0 | °C |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Compression permanent deformation 3 | 23°C,22hr | ASTMD395B | 16 | % |
70°C,22hr | ASTMD395B | 40 | % | |
23°C,22hr | ISO815 | 16 | % | |
70°C,22hr | ISO815 | 40 | % | |
Tensile stress | 100%Strain | ASTMD412 | 5.50 | Mpa |
100%Strain | ISO37 | 5.50 | Mpa | |
300%Strain | ASTMD412 | 9.70 | Mpa | |
300%Strain | ISO37 | 9.70 | Mpa | |
Yield | ISO37 | 36.6 | Mpa | |
Tensile strength | Yield | ASTMD412 | 36.6 | Mpa |
elongation | Break | ASTMD412 | 610 | % |
Break | ISO37 | 610 | % | |
Tear strength 2 | ASTMD624 | 87.6 | kN/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A | ASTMD2240 | 85 | |
Shore A | ISO868 | 85 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Huangdu Index | -- | DIN6167 | <10 | YI |
-- | ASTME313 | <10 | YI |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.