TPU Elastollan® 1195A10 BASF GERMANY
264
- Unit Price:
- $4915 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 148MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Hydrolysis resistance Antibacterial High toughness
- Application Areas:Cable household electrical appl Fitness equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 210°C/10.0kg | ASTMD1238 | 35to65 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | Injection | ASTMD412 | 51.7 | Mpa |
Bending modulus | Injection | ASTMD790 | 52.4 | Mpa |
Taber abraser | ASTMD1044 | 55.0 | mg | |
Abrasion-DIN | DIN53516 | 25 | mm³ | |
Tensile strength at break | ASTM D-412 | 48.3 | Mpa | |
elongation | Break | ASTM D-412 | 450 | % |
tear strength | ASTM D-624 | 140 | kN/m | |
hardness | shoreA | ASTM D-648 | 95 | |
Tensile modulus | ASTM D-638 | 41.4 | Mpa | |
100% tensile stress | ASTM D-412 | 16.5 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
vicat softening point | ASTM D-1525 | 116 | °C | |
Glass transition temperature | 内部方法 | -28.0 | °C | |
Vicat softening temperature | ASTMD1525 | 127 | °C | |
SofteningPoint DMA | 内部方法 | 89 | °C |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
elongation | Break | ASTMD412 | 430 | % |
Tear strength 2 | ASTMD624 | 140 | kN/m | |
Permanent compression deformation | 23°C,22hr | ASTMD395B | 30 | % |
70°C,22hr | ASTMD395B | 45 | % | |
Tensile stress | 100%Strain | ASTMD412 | 17.2 | Mpa |
300%Strain | ASTMD412 | 35.9 | Mpa | |
Tensile strength | ASTMD412 | 39.3 | Mpa |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A | ASTMD2240 | 95 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.75mm | UL94 | HB | |
3.0mm | UL94 | HB |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTM D-792 | 1.14 | g/cm | |
Melt index | ASTM D-1238 | 50 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.