Need Help? Contact Us service@plas.com
Get App

ASA Luran® S ASA 777K UV BK60166 INEOS STYRO KOREA

122
  • Unit Price:
    $2890 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    51MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Density/specific gravityISO11831.07g/cm³
Melt volume flow rate220°C/10.0kgISO113315.0cm3/10min
Shrinkage rateISO294-40.50to0.90%
Water absorption rateSaturation,23°CISO621.7%
Water absorption rateEquilibrium,23°C,50%RHISO620.35%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulusISO527-22300Mpa
Tensile stressYield,23°CISO527-248.0Mpa
Tensile strainYield,23°CISO527-23.3%
TensileCreepModule1hrISO899-11850Mpa
Tensile creep modulus1000hrISO899-11400Mpa
Bending stressISO17870.0Mpa
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature 20.45MPa,AnnealedISO75-2/B101°C
Hot deformation temperature 21.8MPa,AnnealedISO75-2/A97.0°C
Vicat softening temperature--ISO306/A50105°C
Vicat softening temperature--ISO306/B5097.0°C
Linear coefficient of thermal expansionMDISO11359-28.0E-5to1.1E-4cm/cm/°C
thermal conductivityDIN526120.17W/m/K
Electrical performanceTest ConditionTest MethodTest ResultUnit
Surface resistivityIEC600931E+13ohms
Volume resistivityIEC600931E+14ohms·cm
Dielectric constant100HzIEC602503.70
Dissipation factor100HzIEC602500.011
Dissipation factor1MHzIEC602500.024
filmTest ConditionTest MethodTest ResultUnit
Elongation MDBreakISO527-39.0%
Impact performanceTest ConditionTest MethodTest ResultUnit
Charpy Notched Impact Strength -30°CISO1794.0kJ/m²
Charpy Notched Impact Strength 23°CISO17917kJ/m²
Impact strength of cantilever beam gap-30°CISO180/A4.0kJ/m²
Impact strength of cantilever beam gap23°CISO180/A14kJ/m²
hardnessTest ConditionTest MethodTest ResultUnit
Ball pressure hardnessISO2039-180.0Mpa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.