COC ZEONEX® E48R ZEON JAPAN
247
- Unit Price:
- $29514 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 34MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Ozone resistant Oil resistant
- Application Areas:pipeline Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Molding shrinkage rate | ASTM D955 | 1.01 | % | |
Melt index (flow coefficient) | ASTM D1238/ISO 1133 | 25 | g/10min |
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 280°C/2.16kg | JISK6719 | 25 | g/10min |
Water absorption rate | Equilibrium | ASTMD570 | <0.010 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2 | 2500 | Mpa | |
Tensile stress | ISO527-2 | 71.0 | Mpa | |
Tensile strain | Break | ISO527-2 | 10 | % |
Bending modulus | ISO178 | 2500 | Mpa | |
tensile strength | ASTM D638/ISO 527 | 71 | kg/cm²(MPa)[Lb/in²] | |
Bending modulus | ASTM D790/ISO 178 | 2500 | kg/cm²(MPa)[Lb/in²] | |
bending strength | ASTM D790/ISO 178 | 104 | kg/cm²(MPa)[Lb/in²] | |
Tensile modulus | ASTM D638/ISO 527 | 2500 | kg/cm²(MPa)[Lb/in²] | |
Charpy impact strength | ASTM D256/ISO 179 | 21 | kg·cm/cm(J/M)ft·lb/in | |
Tensile elongation at break (elongation at break) | ASTM D638/ISO 527 | 10 | kg/cm²(MPa)[Lb/in²] |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | ASTM D648/ISO 75 | 122 | ℃(℉) | |
Glass transition temperature | JISK7121 | 139 | °C | |
Linear coefficient of thermal expansion | MD | ASTME831 | 6E-05 | cm/cm/°C |
Combustibility (rate) | UL94 | hb |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | ASTM D257/IEC 60093 | 1.0E+16 | Ω.cm |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index | ASTMD542 | 1.531 | ||
Light transmittance | ASTM D1003/ISO 13468 | 93 | % | |
transmissivity | 3000µm | ASTMD1003 | 92.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.