Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
SpiralFlow4.5 | | 内部方法 | 11.0 | CM |
Shrinkage rate 6 | TD | ISO294-4 | 1.3 | % |
Shrinkage rate 6 | MD | ISO294-4 | 1.0 | % |
Water absorption rate | Saturation,23°C | ISO62 | 0.45 | % |
Water absorption rate - saturation | 100°C | ISO62 | 0.55 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile modulus | 23°C | ISO527-2 | 3900 | Mpa |
Tensile stress | Yield,23°C | ISO527-2 | 98.0 | Mpa |
Tensile strain | Break,23°C | ISO527-2 | 30 | % |
Bending modulus | 23°C | ISO178 | 3800 | Mpa |
Bending stress | 23°C7 | ISO178 | 165 | Mpa |
Bending stress | 3.5%Strain,23°C | ISO178 | 125 | Mpa |
Bending stress | 125°C | ISO178 | 85.0 | Mpa |
Bending stress | 175°C | ISO178 | 19.0 | Mpa |
Bending stress | 275°C | ISO178 | 12.5 | Mpa |
Compressive stress | 23°C | ISO604 | 125 | Mpa |
Compressive stress | 120°C | ISO604 | 70.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/Af | 152 | °C |
Glass transition temperature | --8 | ISO11357-2 | 143 | °C |
Glass transition temperature | --9 | ISO11357-2 | 150 | °C |
Melting temperature | | ISO11357-3 | 343 | °C |
Linear coefficient of thermal expansion | MD:<143°C | ISO11359-2 | 4.5E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | MD:>143°C | ISO11359-2 | 1.2E-04 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:<143°C | ISO11359-2 | 5.5E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:>143°C | ISO11359-2 | 1.4E-04 | cm/cm/°C |
thermal conductivity | 23°C10 | ISO22007-4 | 0.29 | W/m/K |
thermal conductivity | 23°C11 | ISO22007-4 | 0.32 | W/m/K |
RTIElec | | UL746 | 260 | °C |
Evolution Calendar intelligent importer | | UL746 | 180 | °C |
RTI | | UL746 | 240 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | 23°C | IEC60093 | 1E+16 | ohms·cm |
Volume resistivity | 125°C | IEC60093 | 1E+15 | ohms·cm |
Volume resistivity | 275°C | IEC60093 | 1E+09 | ohms·cm |
Dielectric strength | 2.00mm | IEC60243-1 | 24 | KV/mm |
Dielectric constant | 23°C,1kHz | IEC60250 | 2.90 | |
Dissipation factor | 23°C,1MHz | IEC60250 | 4E-03 | |
Leakage Trace Index | | IEC60112 | 150 | V |
Filling analysis | Test Condition | Test Method | Test Result | Unit |
---|
Melt viscosity | 400°C | ISO11443 | 350 | Pa·s |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Unscented Izod impact strength | 23°C | ISO180 | 无断裂 | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore hardness | Shore D,23°C | ISO868 | 85 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
Burning wire flammability index | 2.0mm | IEC60695-2-12 | 960 | °C |
Extreme Oxygen Index | --12 | ISO4589-2 | 24 | % |
Extreme Oxygen Index | --13 | ISO4589-2 | 35 | % |
toxicity | COcontent | NES713 | 0.0740 | |
toxicity | CO2content | NES713 | 0.150 | |
toxicity | Totalgases | NES713 | 0.220 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.